This post illustrates a possible sulfide stress cracking mechanisms at the open circuit potential for low alloy steels.
Hydrogen Stress Cracking
Hydrogen diffusion control during stress corrosion cracking of magnesium alloy AZ31B in chloride solutions – Abstract
SCC of AZ31B alloy was studied in NaCl solutions at different potentials and chloride concentrations using the slow strain rate technique. A combination of pre-exposure tests followed by immediate straining or straining after a dry air exposure delay helped to weight the relative importance of anodic damage accumulation versus increased hydrogen charging during open-circuit potential pre-exposure. The dependence of ductility with pre-exposure time and the fracture surface of embrittled samples suggest that hydrogen embrittlement of AZ31B was controlled by hydrogen diffusion.